Notes/Preview
The contents of this course include six recorded presentations from the ACI 2021 Fall Virtual Convention.
• Design and Construction of Residential Concrete Walls with Fiber Reinforcement, by Amir Bonakdar, Euclid Chemical
• Fiber-Reinforced Concrete for Optimized Construction of Light Rail Track Slabs, by Barzin Mobasher, Arizona State University
• Owner’s Perspective for Use of Fibers in Industrial Floor Slabs, by Jason Harris, General Motors
• Innovative SFRC Floors: Research, Design Principle, and Applications, by Hendrik Thooft, Bekaert
• Design and Application of Precast Fiber-Reinforced Concrete Tunnel Lining, by Mehdi Bakhshi, AECOM
• Design and Application of FRC Elevated Slabs, by Giovanni Plizzari, University of Brescia
INSTRUCTIONS: Study the materials included in this module. Then, complete and pass the corresponding 10-question quiz with a score of 80% or higher to receive a certificate for 0.15 CEU (equivalent to 1.5 PDH).
Continuing Education Credit: 0.15 CEU (1.5 PDH)
Approved by AIA and ICC
Access Period: 30 days
Description
The application of fiber-reinforced concrete (FRC) has significantly expanded in the last several years, complimented by the publication of various guides and reports by ACI Committee 544 – Fiber Reinforced Concrete. In this course, project case studies will be presented in which fiber reinforcement has fully or partially replaced reinforcing bars in concrete, allowing optimization of construction time and procedures. Presentations include basics of design for FRC and construction practices. Examples are industrial slabs-on-ground, light-rail track slabs, residential concrete basement walls, precast concrete tunnel segments, elevated concrete slabs with combined fiber and reinforcing bar reinforcement. This course will be useful for students, engineers, contractors, suppliers, testing labs, and government officials.
Document Details
Author: Bonakdar,Mobasher,Harris,Thooft,Bakhshi,Plizzari
Publication Year: 2022
ISBN:
Categories: Construction Practices, Fiber-Reinforced Concrete, Sustainability
Formats: Online Learning
Table of Contents
Learning Objectives
1. Explain the basics and advantages of fiber-reinforced concrete use in slab-on-ground applications when compared to deformed-bar or wire reinforcement.
2. Review case studies of projects that used fiber reinforcement to improve concrete performance.
3. Discuss how fibers in concrete can be used to optimize the construction process, including improving scheduling and increasing production of steel fiber-reinforced slab-on-ground.
4. Identify methods to use steel fibers in combination with deformed-bar reinforcement to design supported slabs on piles or other types of supports.
ERRATA INFO
Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the
Errata page.
Return/Exchange Policy
Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.
Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.
Subscriptions These items are not eligible for return.
Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).